Post-plating treatment: auto parts after plating

(1) Engine cylinder block main bearing bearing hole brush plating processing

After the brush plating, the first and second main bearing bores of the cylinder block are boring. Generally, the boring amount of 0.10 mm can be boring in 2 or 3 times, and the cutting depth should be 0.015 to 0.02 mm.

(2) Crankshaft brush plating treatment

1 water rinse;

2 dry the surface;

3 coated with protective oil;

4 Standard size for grinding to the journal on a crankshaft grinder.

(3) Post-plating treatment of interior and exterior decorative parts

1 water rinse;

2 baked;

3 Check whether the surface has blasting, check whether there is any leakage coating, hammer the coating with no cracks and bulges, and the quality of the brush plating is qualified.

(4) Car wheel hub plating sandwich plating treatment

1 After the size is plated, the water is washed away;

2 drying;

3 oiled.

Global hardware network

Concerned about surprises

Label: Brush Plating Depth of Depth Main Bearing Auto Parts Post Processing

Previous: Bright additive in the production of sulphate electroplated zinc wire Next: After brush plating: post-treatment of brush chrome plating

Spiral Steel Pipe

Anti Corrosion Pipe,Spiral Steel Pipe,Large-Diameter Pipe,Spiral Steel Pipe

Tianyi Steel Pipe Co., Ltd. , http://www.czseamlesspipe.com

This entry was posted in on